top of page

Price 1/m2 incl. VAT Product

Description Classic coffee color Decking 1 side grooves T&G End-Match Pre-primed Reversible dassoCTECH Fused Bamboo
Decking Grade Fused Bamboo
Thickness (mm) 20 mm
Width (mm) 137 mm
Length (mm) 1,850 mm
Density: 1200kg/m³
Moisture Content: 8~12%
Hardness Brinell > 9.5Kg/mm2 [EN1534]
Fire Rating Bf1-s1: EN13501-1
Slip Resistance: Class B (DIN 51097)
Pre-primed Yes - WOCA oil
Modulus of Elasticity: 16700 MPa (GB/T17657-2013
Static Bending Strength: 73,8 MPa (GB/T17657-2013)
Biological Durability: Class 1 (EN335)
Release of Formaldehyde: E1(0.4mg/m²h) (GB/T17657-2013)
Length of Swelling Rate: 0 (DIN EN 15534-1)
Width of Swelling Rate: 0.6% (DIN EN 15534-1)
Fastening Clips & Screws available Yes
Construction Strand
Process or treatment Carbonized and Fused
Binding process Fusion Press
Face/bottom milling One side v-grooved
Binding agent Dynea phenolic resin
Joinery End matched, both side lengths grooved
Board Edges Profile sides rounded 3mm, ends beveled 2mm

dassoCTECH end profile

kr260.00Price
  •  

    dassoCTECH bamboo decking boards

    Environment Friendly Ready for harvest after 4-6 years [compared to up to 100 years forhardwood species] – no deforestation

    CO2 neutral Up to 1 metre growth a day. A giant grass with best marks for ecology.

    Mould Resistance Class 0[DIN EN ISO 846: 1997-10][DIN EN 152: 2011]

    Hard & Durable Durability: Class 1[CEN/TS 15083-1: 2005][EN 350: 2016] Durability: Class 1[CEN/TS 15083-2: 2005][EN 350: 2016]

    Termite Resistance Reticulitermes santonensisDC D(durable)[EN 117] Class 1: AS 5604 (2005)

    Fire Resistance Bf1-s1: EN13501-1 BAL 29: AS 1530.8.1-2007

    Warranty 25 - Year Limited Warranty

    dassoCTECH is crystalized the fibers with CeramiX® particles,impregnated it with phenolic resin ( the same resin found inbowling balls ), then compressed to form Fused Bamboo.Because Fused Bamboo is now fully impregnated withCeramiX® particles that crystalizes the nutrients fromattracting bacteria, fungus, molds or insects, the fibers doesnot rot under exposed environments.

bottom of page